  • n1.jpg

Nickel-plated Flat Wire

1. The coating of the conductor shall be continuous and firm, and the surface of the sample shall be free of oxidation and blackening after the test.2. The coating surface of the conductor should be smooth and continuous, without particles, burrs, mechanical damage and other harmful defects.

Classification:

Details

Product Parameters

Name Model Specifications
Thickness (mm) Width (mm)
Silver-plated copper flat wire BTRY 0.03 -0.30 0.25 -4.50
Nickel-plated copper flat wire BTRN 0.03 -0.30 0.25 -4.50
Alloy flat wire (tin plated, silver plated, nickel plated) BHY 0.03 -0.30 0.25-8.0

 

Raw materials and product standards 1. Silver plated copper wire GB/T3135
2. Tinned copper wire GB/T 4910
3. Nickel plated copper wire GB/T11019
4. Copper for electrical purposes GB/T3953

 

Resistivity Model (Ωmm²/m at 20°C)
BTRY ≤ 0.017241
BTRN ≤ 0.019157
BHY ≤ 0.02960

 

Mechanical properties Model Tensile strength (N/mm) not less
soft state hard state
BTRY 196 /
BTRN 196 /
BHY Depending on the specific alloy Depending on the specific alloy

 

Plating 1. The coating of the conductor shall be continuous and firm, and the surface of the sample shall be free of oxidation and blackening after the test.
2. The coating surface of the conductor should be smooth and continuous, without particles, burrs, mechanical damage and other harmful defects.

 

Inspection rules and test methods Product inspection: incoming inspection → process inspection → finished product inspection, finished product inspection qualified factory each batch of products with quality inspection certificate.

 

Inspection Items Serial Number Project Test Method
1 Silver content and coating thickness Coating tester
2 Monofilament Diameter and Tolerances micrometer micrometer
3 Appearance Normal Visual Examination
4 Plating continuity GB/T4909.9
5 Mechanical properties GB/T 4909.3
6 Resistivity GB/T3048.2